环境性能:PPS耐辐射性好。耐化学腐蚀性好,仅次于F4。不耐氯代联苯及氧化性酸,氧化剂等。
供应PPS美国菲利浦R-4-230BL,R-4-230NA阻燃玻纤增强;
PPS R-4-230BL 菲利浦石油国际有限公司 物性数据 |
暂无此原料描述部分┄ |
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |
基本性能 | 密度 | --- | ASTM D-792 | 1.65 | g/10min |
吸水率 | --- | ASTM D-570 | 0.05 | % | |
物理性能 | 颜色 | --- | --- | Black | --- |
机械性能 | 抗拉强度 | --- | ASTM D-638 | 23.0 | Ksi |
伸长率 | --- | ASTM D-638 | 1.2 | % | |
抗折强度 | --- | ASTM D-790 | 30.0 | Ksi | |
抗拉模数 | --- | ASTM D-790 | 2.1 | Msi | |
抗压强度 | --- | ASTM D-695 | 35.0 | Ksi | |
IZOD冲击强度1/8inch有缺1/8inch无缺 | --- | ASTM D-256ASTM D-256 | 1.57.0 | ft.lbf/inft.lbf/in | |
电气性能 | 绝缘破坏电压 | --- | ASTM D-149 | 500 | V/mil |
介电常质数 | 1KHz | ASTM D-150 | 4.0 | --- | |
介电常质数 | 1MHz | ASTM D-149 | 3.9 | --- | |
捐耗因素 | 1KHz | ASTM D-150 | 0.002 | --- | |
损耗因素 | 1MHz | ASTM D-150 | 0.003 | --- | |
体积电阻率 | --- | ASTM D-257 | 2×1015 | Ω.cm | |
耐电弧 | --- | ASTM D-495 | 125 | Sec | |
绝缘电阻 | 90℃,48hrs | --- | 1×1011 | Ω | |
电弧踪迹 | --- | UL 746A | 14.0 | in/min | |
CTI踪迹 | --- | UL 746A | 175 | V | |
热 性 能 | 燃烧性 | --- | UL 94 | V-0/5VA | --- |
热变形温度 | --- | ASTM D-648 | >500 | °F | |
UL温度指数 | --- | UL | 200/220 | ℃ |
PPS塑料成型性能好,吸湿小,宜干燥后成型。.流动性介于ABS和PC之间,凝固快,收缩小,易分解,
选用较高的注射压力和注射速度。模温取100-150度。主流道锥度应大,流道应短。